3d printing filament basf innofil gf30 Search Results


90
BASF pa 6.6 gf30 ultramid a3wg6
Investigated polymers with filler content <t> (GF30 </t> = 30 wt.% glass fiber) and recommended processing temperatures (according to Moldflow material data base in the software version 2016).
Pa 6.6 Gf30 Ultramid A3wg6, supplied by BASF, used in various techniques. Bioz Stars score: 90/100, based on 1 PubMed citations. ZERO BIAS - scores, article reviews, protocol conditions and more
https://www.bioz.com/product/3d+printing+filament+basf+innofil+gf30/3d+printing+filament+basf+innofil+gf30/pmc08472572-64-3-8
Average 90 stars, based on 1 article reviews
pa 6.6 gf30 ultramid a3wg6 - by Bioz Stars, 2026-09
90/100 stars
  Buy from Supplier

Image Search Results


Investigated polymers with filler content  (GF30  = 30 wt.% glass fiber) and recommended processing temperatures (according to Moldflow material data base in the software version 2016).

Journal: Polymers

Article Title: Influence of the Mold Material on the Injection Molding Cycle Time and Warpage Depending on the Polymer Processed

doi: 10.3390/polym13183196

Figure Lengend Snippet: Investigated polymers with filler content (GF30 = 30 wt.% glass fiber) and recommended processing temperatures (according to Moldflow material data base in the software version 2016).

Article Snippet: PA 6.6 , GF30 , Ultramid A3WG6 , BASF , 290 , 85 , 195.

Techniques: Software

Temperature coefficient (TC), cycle times, and cycle time reduction (CTR) for the investigated polymers for 1 mm part thickness.

Journal: Polymers

Article Title: Influence of the Mold Material on the Injection Molding Cycle Time and Warpage Depending on the Polymer Processed

doi: 10.3390/polym13183196

Figure Lengend Snippet: Temperature coefficient (TC), cycle times, and cycle time reduction (CTR) for the investigated polymers for 1 mm part thickness.

Article Snippet: PA 6.6 , GF30 , Ultramid A3WG6 , BASF , 290 , 85 , 195.

Techniques:

Temperature coefficient (TC), cycle times, and cycle time reduction (CTR) for the investigated polymers for 3 mm part thickness.

Journal: Polymers

Article Title: Influence of the Mold Material on the Injection Molding Cycle Time and Warpage Depending on the Polymer Processed

doi: 10.3390/polym13183196

Figure Lengend Snippet: Temperature coefficient (TC), cycle times, and cycle time reduction (CTR) for the investigated polymers for 3 mm part thickness.

Article Snippet: PA 6.6 , GF30 , Ultramid A3WG6 , BASF , 290 , 85 , 195.

Techniques:

Deformation results of the open side of the box for the investigated polymers for 1 mm and 3 mm part thickness for both mold materials.

Journal: Polymers

Article Title: Influence of the Mold Material on the Injection Molding Cycle Time and Warpage Depending on the Polymer Processed

doi: 10.3390/polym13183196

Figure Lengend Snippet: Deformation results of the open side of the box for the investigated polymers for 1 mm and 3 mm part thickness for both mold materials.

Article Snippet: PA 6.6 , GF30 , Ultramid A3WG6 , BASF , 290 , 85 , 195.

Techniques: